The reduction from the Barcol hardness following 10 wt.% is often attributed for the lousy wettability amongst the fibres as well as the matrix bringing about agglomeration because the fibre weight proportion raises upto 15 wt.%. From fifteen wt.%, the values of hardness raises consistently upto 50 wt.% as a consequence of far more even distributio